Originally Posted by Bonnar_Bloke
Hi MF,

What is the "tan nectar" you refer to ?

Normally you would use washing Soda and also place Anodes into the bath and then hooking up a battery charger to both the anodes (two of) and the job, thus finishing the process in less than 24 hours and not a month as you suggest.

Cheers,
BB.
Hello Bonnar_Bloke, Speedie and AVB,
BB, I was referring to the sugar cane molasses you mix with the water. I will try the electrode method when I run out out of molasses.
Speedie, what do you do once the items come out?
AVB I don't know about the paint, but any rust showing through will certainly be targeted.


Ahh, if only victa had kept producing the thumblatch catcher series, they would be in better shape today!