Hi all, DO NOT use stainless steel as your sacrificial anode in the conductive solution, as this will produce Hexavalent chromium which is a genotoxic carcinogen. I use black 2 mm sheet steel in a 60 ltr tube with soldered 15 amp house wire conecting the anodes together, so u have wall to wall line of sight a fused charger 12/24 volt 30 amp .... Sodium Carbonate works best as the conductive solution u can find this ingredient in a product called lectic its often used as a water softner comes in crystal and powder form cheers steve.